有高的強(qiáng)度、韌度和良好的淬透性和抗過熱的穩(wěn)定性,但白點(diǎn)敏感性高,有回火脆性。焊接性較差,焊前需經(jīng)高溫預(yù)熱,焊后需消除應(yīng)力,經(jīng)調(diào)質(zhì)后使用。
化學(xué)成分
碳C 0.37~0.44
硅Si 0.17~0.37
錳Mn0.50~0.80
硫S 允許殘余含量≤0.025
磷P 允許殘余含量≤0.025
鉻Cr 0.60~0.90
鎳Ni 1.25~1.65
銅Cu 允許殘余含量≤0.25
鉬Mo0.15~0.25
自由鍛件供應(yīng)哪家好,就找唐山盛通鍛造有限公司。
It has high strength, toughness, good hardenability and resistance to overheating, but has high white point sensitivity and temper brittleness. Poor weldability, preheating before high temperature, need to eliminate stress after welding, after quenching and tempering.
chemical composition
Carbon C 0.37~0.44
Silicon Si 0.17~0.37
Manganese Mn 0.50~0.80
Sulfur S allows residual content ≤0.025
Phosphorus P allows residual content ≤0.025
Chromium Cr 0.60~0.90
Nickel Ni 1.25~1.65
Copper Cu allows residual content ≤ 0.25
Molybdenum Mo0.15~0.25